性能項目 | 測試條件 | 測試方法 | 數(shù)值/描述 | 單位 | |
機(jī)械性能 | 拉伸強(qiáng)度(引張強(qiáng)度) | ASTM D638/ISO 527 | 370(5250) | kg/cm2(MPa)[Lb/in2] | |
斷裂伸長率 | ASTM D638/ISO 527 | -- | % | ||
拉伸模量 | ASTM D638/ISO 527 | -- | kg/cm2(MPa)[Lb/in2] | ||
拉伸屈服伸長率(延伸率) | ASTM D638/ISO 527 | 40 | % | ||
拉伸斷裂伸長率(延伸率) | ASTM D638/ISO 527 | -- | % | ||
彎曲模量(彎曲彈性率) | ASTM D790/ISO 178 | 20000(28000) | kg/cm2(MPa)[Lb/in2] | ||
彎曲強(qiáng)度 | ASTM D790/ISO 178 | 560(8000) | kg/cm2(MPa)[Lb/in2] | ||
洛氏硬度 | ASTM D785 | R-100 | |||
IZOD 缺口沖擊強(qiáng)度 | 1/4" 23℃ | ASTM D256/ISO 179 | -- | kg·cm/cm(J/M)ft·lb/in | |
1/4" -30℃ | ASTM D256/ISO 179 | 37(6.9) | kg·cm/cm(J/M)ft·lb/in | ||
1/8" 23℃ | ASTM D256/ISO 179 | -- | kg·cm/cm(J/M)ft·lb/in | ||
1/8" -30℃ | ASTM D256/ISO 179 | 44(8.1) | kg·cm/cm(J/M)ft·lb/in | ||
Charpy沖擊強(qiáng)度 | 23℃ (缺口) | ASTM D256/ISO 179 | -- | kg·cm/cm(J/M)ft·lb/in | |
-30℃(缺口) | ASTM D256/ISO 179 | -- | kg·cm/cm(J/M)ft·lb/in | ||
23℃(無缺口) | ASTM D256/ISO 179 | -- | kg·cm/cm(J/M)ft·lb/in | ||
-30℃(無缺口) | ASTM D256/ISO 179 | -- | kg·cm/cm(J/M)ft·lb/in | ||
物性性能 | 比重(密度) | ASTM D792/ISO 1183 | 1.03 | ||
成型收縮率 | ASTM D955 | -- | % | ||
熔融指數(shù)(流動系數(shù)) | 200℃/5kg | ASTM D1238/ISO 1133 | 0.4 | g/10min | |
220℃/10kg | ASTM D1238/ISO 1133 | 4.5 | g/10min | ||
吸水率 23℃/24H | ASTM D570/ISO 62 | -- | % | ||
熱性能 | 熱變形溫度 | 退火 | ASTM D648/ISO 75 | 96(205) | ℃(℉) |
未退火 | ASTM D648/ISO 75 | 86(187) | ℃(℉) | ||
維卡軟化點 | ASTM D1525/ISO R306 | -- | ℃(℉) | ||
熔點 | - | -- | ℃(℉) | ||
燃燒性(率) | UL94 | 1.6mmHB | |||
線性膨脹系數(shù) | ASTM D696/ISO 11359 | -- | mm/mm.℃ | ||
加工條件 | 干燥條件 | 80°C下烘料約2~3小時 | |||
加工溫度 | 射嘴 | 190~250°C | ℃ | ||
料筒前段 | 220~250 °C | ℃ | |||
料筒中段 | 210~240 | ℃ | |||
料筒后段 | 190~210 | ℃ | |||
熔體溫度 | -- | ℃ | |||
模具溫度 | -- | ℃ | |||
壓力 | 注塑壓力 | -- | Mpa | ||
保壓壓力 | -- | Mpa | |||
背壓 | -- | Mpa | |||
螺桿轉(zhuǎn)速 | -- | rpm | |||
其他 | 備注 | 在射出周期中勿將熱融膠長期停留在加熱管中 | |||
顏色 | -- | ||||
特性 | 超高耐沖擊 | ||||
用途 | 擠出管材 / 家具 / 大件容器等 |
ABS 臺灣奇美 PA-709S 超高耐沖擊