廠家(產(chǎn)地):日本東麗
加工級別:注塑級
牌號:A504
特性級別:耐高溫
耐高溫PPS A504 日本東麗PPS 物性數(shù)據(jù)表
①原料描述部分
規(guī)格級別:玻璃纖維增強級
外觀顏色:---
用途概述:---
備注說明:特性:標(biāo)準(zhǔn)
②原料技術(shù)數(shù)據(jù)
|
|||||||||||||
性能項目
|
試驗條件[狀態(tài)]
|
測試方法
|
測試數(shù)據(jù)
|
數(shù)據(jù)單位
|
|||||||||
基本性能
|
吸水率
|
---
|
ASTM D-570
|
0.02
|
%
|
||||||||
物理性能
|
比重
|
---
|
ASTM D-792
|
1.70
|
---
|
||||||||
|
---
|
|
|
|
|||||||||
流動長
|
320℃,98MPa,1mm厚
|
東麗法
|
124
|
×10-3m
|
|||||||||
機械性能
|
引張強度
|
---
|
ASTM D-638
|
155
|
MPa
|
||||||||
拉伸強度
|
---
|
ASTM D-638
|
1.6
|
%
|
|||||||||
彎曲強度
|
---
|
ASTM D-790
|
205
|
MPa
|
|||||||||
彎曲彈性體
|
---
|
ASTM D-790
|
13.7
|
GPa
|
|||||||||
斷裂強度
|
---
|
ASTM D-732
|
75
|
---
|
|||||||||
|
---
|
|
|
|
|||||||||
硬度
|
---
|
ASTM D-785
|
120
|
洛氏
|
|||||||||
摩耗
|
---
|
ASTM D-1044
|
50
|
mg/1000回
|
|||||||||
摩擦系數(shù)
|
對鋼
|
ASTM D-1894
|
0.25
|
---
|
|||||||||
限界PV值
|
---
|
東麗法
|
東麗法
|
kj/m2.hr
|
|||||||||
電氣性能
|
耐電弧性W電級
|
---
|
ASTM D-495
|
127
|
秒
|
||||||||
體積固有抵抗
|
---
|
ASTM D-257
|
1016
|
Ω.m
|
|||||||||
絕緣破壞電壓
|
---
|
ASTM D-149
|
21
|
MV/m
|
|||||||||
誘電率
|
106Hz
|
ASTM D-150
|
3.8
|
---
|
|||||||||
誘電正接
|
106Hz
|
ASTM D-150
|
0.002
|
---
|
|||||||||
熱 性 能
|
融點
|
---
|
DSC
|
278
|
℃
|
||||||||
熱變形溫度
|
1.82MPa
|
ASTM D-648
|
>260
|
℃
|
|||||||||
|
---
|
|
|
|
|||||||||
燃燒性
|
---
|
UL-94
|
V-0
|
---
|