③原料技術數(shù)據(jù)
性能項目 | 試驗條件[狀態(tài)] | 測試方法 | 測試數(shù)據(jù) | 數(shù)據(jù)單位 | |
基本性能 | 吸水率 | 飽和(23℃) | ASTM D-570 | 4.6 | % |
吸水率 | 24小時浸漬(23℃) | ASTM D-570 | 0.5 | % | |
物理性能 | 比重 | ASTM D-792 | 1.35 | ||
機械性能 | 洛氏硬度R | DAM | ASTM D-785 | R122 | |
撓曲模量 | 23℃,50%RH | ASTM D-790 | 5516 | MPa | |
撓曲模量 | 23℃,DAM | ASTM D-790 | 6895 | MPa | |
埃佐沖擊強度 | 23℃,50%RH | ASTM D-256 | 128 | j/m | |
斷裂伸長率 | 23℃,50%RH | ASTM D-638 | 4 | % | |
擠剪強度 | 23℃,DAM | ASTM D-732 | 72 | MPa | |
洛氏硬度M | 50%RH | ASTM D-785 | M90 | ||
洛氏硬度M | DAM | ASTM D-785 | M96 | ||
斷裂伸長率 | 23℃,DAM | ASTM D-638 | 3 | % | |
洛氏硬度R | 50%RH | ASTM D-785 | R118 | ||
泰伯磨耗量 | 50%RH | 36 | cycles | ||
撓曲強度 | 23℃,DAM | ASTM D-790 | 228 | MPa | |
埃佐沖擊強度 | 23℃,DAM | ASTM D-256 | 128 | j/m | |
拉伸強度 | 23℃,DAM | ASTM D-638 | 151.6 | MPa | |
拉伸強度 | 23℃,50%RH | ASTM D-638 | 110.3 | MPa | |
電氣性能 | 體積電阻率 | DAM | ASTM D-257 | 1014 | ohm-cm |
介電強度 | (分步法)DAM | ASTM D-149 | 510 | volts/mil | |
損耗因數(shù) | DAM@106Hz赫 | ASTM D-150 | 0.02 | ||
介電強度 | RH | ASTM D-149 | 255 | volts/mil | |
介電常數(shù) | DAM@103Hz赫 | ASTM D-150 | 4.2 | ||
損耗因數(shù) | DAM@103Hz赫 | ASTM D-150 | 0.02 | ||
體積電阻率 | RH | ASTM D-257 | 109 | ohm-cm | |
介電強度 | DAM | ASTM D-149 | 630 | volts/mil | |
介電常數(shù) | DAM@106Hz赫 | ASTM D-150 | 3.4 | ||
熱性能 | 熱畸變溫度 | 1.8MPa | ASTM D-648 | 246 | ℃ |
線性熱膨脹系數(shù) | ASTM D-696 | 1.8×10-5 | m/m/℃ | ||
熔點 | 50%RH | ASTM D-789 | 255 | ℃ | |
熔點 | DAM | ASTM D-789 | 255 |
℃ |